Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Dimethyl sebacate | HCID 7829 | — |
| Edukt | Trimethyl Phosphate | HCID 10541 | — |
| Edukt | Oxo(oxostibanyloxy)stibane | HCID 27652 | — |
| Edukt | Dimethyl-2,6-naphthalenedicarboxylate | HCID 61225 | — |
| Katalysator | Manganese acetate tetrahydrate | HCID 93021 | — |
| Lösungsmittel | Ethylene Glycol | HCID 174 | — |
| Lösungsmittel | Methanol | HCID 887 | — |
| Produkt | Sebacic Acid | HCID 5192 | — |
Reaktionsschritte
Dimethyl 2,6-naphthalenedicarboxylate and dimethyl sebacate were dispersed in ethylene glycol. Then, 0.029 part of manganese acetate tetrahydrate, 0.028 parts of antimony trioxide and 0.1% of spherical silica particles having a mean particle size of 0.3 μm were added to 100 parts of the total of dimethyl 2,6-naphthalenedicarboxylate and dimethyl sebacate, and heated with stirring to conduct the reaction. The temperature was elevated to 235° C. while removing methanol produced as a by-product. After the by-production of methanol was completed, 0.03 part of trimethyl phosphate was added thereto. Then, the pressure was reduced to 0.3 Torr while elevating the temperature to 285° C., thereby conducting the polymerization. Dyes described in JP-A-7-168309, compounds 1-6 and I-24, were each further added to the solid matter in an amount of 54 ppm. The copolymerization ratio of sebacic acid (SA) and the intrinsic viscosity of a polyester thus obtained are shown in Table II-1.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US06518004B2 |
|---|
| Quelldatensatz | uspto-grants-2003_02 |
|---|
| ORD ID | ord-be10107388c34ce9b8324216b15c00ad |
|---|