Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Methane | HCID 297 | — |
| Edukt | Cetylpyridinium Chloride | HCID 31239 | — |
| Produkt | Benzene, ethenyl-, polymer with 1,3-butadiene | HCID 62697 | — |
Reaktionsschritte
A toner was prepared by extrusion of the above polymer, 92 percent, 6 percent of REGAL 330® carbon black and 2 percent of CPC (cetyl pyridinium chloride charge additive) followed by micronization to 10 microns. The minimum fix temperature of the toner was 230° F. as determined by no cracking of the fused toner images as a result of a 180 degrees paper crease test (paper folded 180 degrees, visually observed the breadth of cracking at crease) and the minimum fix temperature of the toner was 230° F. when no appreciable, for example a peppered, toned image was removed with SCOTCH® Tape Magic 810, and the hot offset temperature was 320° F. where the toned image sticks to silicone roll fuser as indicated herein. When fused, toner images were observed to offset from paper onto a silicone fuser roll, and then was imprinted onto the same paper or subsequent papers. The hot offset temperature, where the toner failed to release from the fuser roll, was 300° F.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US05324611 |
|---|
| Quelldatensatz | uspto-grants-1994_06 |
|---|
| ORD ID | ord-f3c1f3c7ea234e8ea232d03deb4c1eb4 |
|---|