Hydrochloric Acid → 2-Phenyl-3-oxazoline
Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|---|---|---|
| Edukt | Hydrochloric Acid | HCID 313 | — |
| Edukt | Sodium Hydroxide | HCID 14798 | — |
| Edukt | Perchloric Acid | HCID 24247 | — |
| Edukt | 2-Phenyl-2-oxazoline | HCID 244030 | — |
| Produkt | 2-Phenyl-3-oxazoline | HCID 15031923 | 88% |
Reaktionsschritte
50 g of 2-phenyl-3-oxazoline are polymerized at the temperature of 150° C. for 40 minutes in the presence of an equimolar complex of perchloric acid with 2-phenyl-2-oxazoline taken in the ratio of the monomer to the initiator equal to 100:1. The resulting poly-N-benzoylethylenimine is hydrolyzed first with an aqueous solution of hydrochloric acid at reflux. The thus-prepared polymer is boiled in a solution of caustic soda. Linear polyethylenimine is dried over phosphorus pentoxide to give 12.8 g of an anhydrous polymer; the yield is 88%, intrinsic viscosity of the polymer [η]20 =0.18 dl/g (abs.alcohol) which corresponds to the molecular mass of 5,000.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patentnummer | US04467115 |
| Quelldatensatz | uspto-grants-1984_08 |
| ORD ID | ord-6185abd091dc46a392e4c94852264d17 |
| Quellennotiz | uspto-grants-1984_08 |