HuagongsheHuagongshe Chemie-Druckbericht · Nur für Forschungszwecke
Acrylamide → Isooctyl Acrylate Acrylamide Vinyl Acetate
Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|---|---|---|
| Edukt | Acrylamide | HCID 6579 | — |
| Edukt | Vinyl Acetate | HCID 7904 | — |
| Edukt | 2,2'-Azobis(2-methylbutyronitrile) | HCID 93079 | — |
| Edukt | Isooctyl acrylate | HCID 165746 | — |
| Lösungsmittel | Methanol | HCID 887 | — |
| Lösungsmittel | Ethyl Acetate | HCID 8857 | — |
| Produkt | Isooctyl Acrylate Acrylamide Vinyl Acetate | HCID 86608178 | — |
Reaktionsschritte
A master batch was prepared by mixing isooctyl acrylate (1233.75 g), acrylamide (118.125 g), vinyl acetate (337.500 g) and 2,2'-azobis(2-methylbutanenitrile) (1.6875 g). A portion (225.475 g) of the master batch, ethyl acetate (257.7) and methanol (28.6 g) were placed in a 1 liter amber bottle. The mixture was deoxygenated by purging with nitrogen (1 L/min) for 2 minutes. The bottle was sealed and placed in a rotating water bath at 57° C. for 24 hours. The bottle was removed, opened, and then charged with ethyl acetate (214.8 g) and methanol (23.8 g). The contents were mixed until uniform (usually overnight). The percent solids of the resulting copolymer solution was 26.4. The inherent viscosity was 1.47 dl/g in ethyl acetate at 0.15 g/dl.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patentnummer | US06132760 |
| Quelldatensatz | uspto-grants-2000_10 |
| ORD ID | ord-b7c1d11cac234d47ab970ff6188f6e54 |
| Quellennotiz | uspto-grants-2000_10 |