Reaktionsgleichung

Beteiligte Stoffe

RolleNameHCIDEinwaage
EduktGlycolic AcidHCID 757—
Edukt2-ethylhexanoic acid tin(II) saltHCID 9318—
Eduktepsilon-CAPROLACTONEHCID 10401—
EduktGlycolideHCID 65432—
ProduktPoliglecaproneHCID 65431—

Reaktionsbedingungen

Temperatur150 °C

Reaktionsschritte

Glycolide (0.21 moles) was mixed with ε-caprolactone (4.0 moles) and a catalytic amount of stannous octoate (0.8 mole) and glycolic acid (0.40 moles). The system was heated to 150° C. and was stirred at this temperature for 14 hours. At the conclusion of the reaction, the unreacted monomer was removed by heating at 120° C. under reduced pressure for 1 hour. The resulting polymer had a peak melting temperature of 54.3° C. as measured by DSC.

Herkunft & Nachweise

DOI10.6084/m9.figshare.5104873.v1
PatentnummerUS06299631B1
Quelldatensatzuspto-grants-2001_10
ORD IDord-515a6a6c9ec040f88ec84ca01eb6da11
Quellennotizuspto-grants-2001_10