HuagongsheHuagongshe Chemie-Druckbericht · Nur für Forschungszwecke
Acrylamide → Isooctyl Acrylate Acrylamide Vinyl Acetate
Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|---|---|---|
| Edukt | Acrylamide | HCID 6579 | — |
| Edukt | Vinyl Acetate | HCID 7904 | — |
| Edukt | 2,2'-Azobis(2,4-dimethylvaleronitrile) | HCID 91537 | — |
| Edukt | Isooctyl acrylate | HCID 165746 | — |
| Lösungsmittel | Methanol | HCID 887 | — |
| Lösungsmittel | Ethyl Acetate | HCID 8857 | — |
| Lösungsmittel | Ethylacetate methanol | HCID 21584119 | — |
| Produkt | Isooctyl Acrylate Acrylamide Vinyl Acetate | HCID 86608178 | — |
Reaktionsschritte
A master batch was prepared by combining isooctyl acrylate (621.0 g), acrylamide (41.4 g), vinyl acetate (165.6 g), 2,2'azobis(2,4-dimethylpentanenitrile) (1.656 g, VAZO™ 52, DuPont), ethyl acetate (884.5 g) and methanol (87.48 g). A portion (400 g) of the resulting solution was placed in a one quart (0.95 L) amber glass bottle. The bottle was purged for 2 minutes with nitrogen at a flow rate of 1 L/min. The bottle was sealed and placed in a rotary water bath at 45° C. for 24 hours to effect essentially complete polymerization. The copolymer was diluted with ethyl acetate: methanol (90:10 v/v) to 26.05% solids and had an inherent viscosity of 1.27 deciliter/gram in ethyl acetate at 0.15 g/deciliter.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patentnummer | US05614210 |
| Quelldatensatz | uspto-grants-1997_03 |
| ORD ID | ord-f7a89e0d666f4ea1b31e9d1dd69fc52f |
| Quellennotiz | uspto-grants-1997_03 |