참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|
| 반응물 | Hydrochloric Acid | HCID 313 | — |
| 반응물 | Itaconic acid | HCID 811 | — |
| 반응물 | Acrylic Acid | HCID 6581 | — |
| 용매 | Water | HCID 962 | — |
| 생성물 | 2-Methylidenebutanedioic acid--prop-2-enoic acid (1/1) | HCID 161509 | 67.9% |
반응 단계
Acrylic acid (1050.0 g, 14.571 moles), itaconic acid (210.64 g, 1.6190 moles), Wako V-50 (4.3919 g, 16.19 millimole), and 7.9 liters of water, which has been acidified to pH 2.0 with hydrochloric acid, are added to a 22 liter three-necked round-bottomed flask fitted with a thermometer, a mechanical stirrer, and gas inlet/outlet adapter capable of bubbling gas through a liquid in the flask and venting it. The solution is deaerated by passage of nitrogen gas and is then placed under an atmosphere of nitrogen. The solution is heated to 55° C. and maintained at this temperature for 15 hours. The viscous solution of copolymer is cooled to ambient temperature and is freeze dried to give 1,222.1 g of poly(acrylic acid-itaconic acid) copolymer as a colorless solid. The mass average molecular weight, as determined by low angle laser light scattering on a dialyzed portion in 0.2 Molar sodium chloride in water (refractive index=1.3344, dn /dc --0.1683), is 711,700.
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 특허 번호 | US05213789 |
|---|
| 출처 데이터셋 | uspto-grants-1993_05 |
|---|
| ORD ID | ord-9cee501332134035a255b7b6dfad059d |
|---|
| 출처 메모 | uspto-grants-1993_05 |
|---|