Huagongshe화공사 화학 정보 인쇄 보고서 · 연구 참고용
Pyromellitic dianhydride → Acetic Anhydride
참여 물질
| 역할 | 이름 | HCID | 투입량 |
|---|---|---|---|
| 반응물 | Pyromellitic dianhydride | HCID 6966 | — |
| 반응물 | Dimethylacetamide | HCID 31374 | — |
| 반응물 | 5,5'-Bi-2-benzofuran-1,1',3,3'-tetrone | HCID 75494 | — |
| 생성물 | Acetic Anhydride | HCID 7918 | — |
| 생성물 | 3-Methylpyridine | HCID 7970 | — |
반응 단계
Polymer was made at room temperature by adding 3,4′-ODA, PPD, BPDA, and PMDA with stirring in DMAc in quantities to make polymers with compositions between 5 and 14 mole % BPDA and between 5 and 21 mole % PPD. The remaining monomers were PMDA as the dianhydride and 3,4′-ODA as the diamine. The polymers were each cast on a substrate and converted in a bath of 50 volume % acetic anhydride and 50 volume % beta-picoline, at room temperature, to form a gel film. The gel film was restrained and heated in an oven to dry and cure at 300° C. for 60 minutes, and then heated in 400° C. oven for 5 minutes. The properties were as follows:
출처 및 근거
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| 특허 번호 | US06956098B2 |
| 출처 데이터셋 | uspto-grants-2005_10 |
| ORD ID | ord-4934ef4e9f334061aa924d7e01e66895 |
| 출처 메모 | uspto-grants-2005_10 |