HRID1689583

反应详情

EQUATION

反应方程式

HRID 1689583 的结构方程式

PROCEDURE

实验过程

An SiON passivation layer, e.g., 104 in FIGS. 1A and 1B, can be deposited in MOCVD mode using reactants SiCl4, NH3, N2O, or ozone appropriately diluted in a nitrogen carrier at approximately 650 C˜750 C. Such a layer could also be formed in ALD mode with cycles of SiCl4 at approximately 400 C˜450 C and NH3-N20-N2 or NH3-O3-N2 at approximately 650 C˜700 C while maintaining appropriate gas pressures of SiCl4, NH3, and N2O to achieve desired film composition at a slow deposition rate less than 0.1 nm/sec.

WORKUP

后处理

  1. additionappropriately diluted in a nitrogen carrier at approximately 650 C˜750 C