十八水合硫酸铝 → 硫酸铝

HRID 237170

反应方程式

HRID 237170 反应方程式
O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.O.[S:19]([O-:23])([O-:22])(=[O:21])=[O:20].[Al+3:24].[S:25]([O-:29])([O-:28])(=[O:27])=[O:26].[S:30]([O-:34])([O-:33])(=[O:32])=[O:31].[Al+3]>O>[S:19]([O-:23])([O-:22])(=[O:21])=[O:20].[Al+3:24].[S:25]([O-:29])([O-:28])(=[O:27])=[O:26].[S:30]([O-:34])([O-:33])(=[O:32])=[O:31].[Al+3:24]

参与物

3

实验过程

To the aqueous polymer mixture was added 1.0 g aluminum sulfate octadecahydrate (Sigma Aldrich, Wis.) in 50 mL deionized water. The polymer mixture was then mixed for 30 minutes to provide a crosslinked polymer gel.

后处理

  1. additionThe polymer mixture was then mixed for 30 minutes
  2. customto provide a crosslinked polymer gel

来源与证据

ORD记录
ord-4099d1be7b444480aa6230029cba152d
来源数据集
uspto-grants-2014_02
专利号
US08641869B2

关联笔记