参与物
| 角色 | 名称 | HCID | 投料 |
|---|
| 反应物 | 对苯二酚 | HCID 785 | — |
| 反应物 | 苯酚 | HCID 996 | — |
| 反应物 | 2-甲基-2-丙烯酸的均聚物 | HCID 4093 | — |
| 反应物 | 3A,4,7,7A-四氢化-4,7-亚甲基-1H-茚的均聚物 | HCID 6492 | — |
| 反应物 | 乙基三苯基醋酸膦 | HCID 94470 | — |
| 溶剂 | 苯乙烯 | HCID 7501 | — |
| 产物 | 1,2-二乙烯基苯 | HCID 66666 | — |
反应步骤
A reactor is charged with 600 g of an epoxy resin prepared from dicyclopentadiene and phenol having an average functionality of about 3.2 and an epoxide equivalent weight (EEW) of 265. The resin is heated at 120° C. for 1 hour with 0.43 g of a 70 weight percent methanolic solution of ethyltriphenylphosphonium acetate.acetic acid complex catalyst with a nitrogen sparge. To the resulting mixture is added 200 g of the diglycidyl ether of bisphenol A having an EEW of 179 thereby forming a homogeneous solution having an EEW of 208. The mixture of epoxy resins is reacted catalytically with a stoichiometric equivalent amount (322 g) of glacial methacrylic acid in the presence of air and 400 ppm hydroquinone at 100° C. to 115° C. until a 1.1% acid concentration is reached. The vinyl ester resin is dissolved in 508 g of styrene and 127 g of divinyl benzene to yield a blend containing about 36 percent monomeric diluent by weight. The diluent contained 80% by weight styrene and 20% by weight divinylbenzene.
来源与证据
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| 专利号 | US04824500 |
|---|
| 来源数据集 | uspto-grants-1989_04 |
|---|
| ORD ID | ord-61b961003bca40aa8f4328879d0b5e2c |
|---|
| 来源说明 | uspto-grants-1989_04 |
|---|