Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Carbon Dioxide | HCID 280 | — |
| Edukt | Calcium | HCID 5460341 | — |
| Edukt | Magnesium | HCID 5462224 | — |
| Edukt | Calciumoxide | HCID 6850728 | — |
| Edukt | Magnesium monoxide | HCID 6850729 | — |
| Lösungsmittel | Water | HCID 962 | — |
| Produkt | Magnesium bicarbonate | HCID 102204 | — |
| Produkt | Calcium bicarbonate | HCID 10176262 | — |
Reaktionsschritte
The roasting process of magnesium or/and calcium minerals is that the minerals are roasted for 1˜5 hours at 700˜1000° C. The process of digestion is that water is added into magnesium oxide and/or calcium oxide obtained after roasting to digest at 50˜95° C., for 0.5˜5 hours, according to the weight ratio of the liquid to solid: 1˜5:1 (calculated by the weight of water and magnesium oxide and/or calcium oxide), and then water is added to form slurry based on the weight ratio of the liquid to solid: 10˜200:1 (calculated by weight of water and magnesium oxide and/or calcium oxide). The process of carbonization is that the slurry is carbonized by carbon dioxide gas after digestion, with reaction temperature controlled at 0˜50° C. and reaction time 0.1˜5 hours. Pure aqueous solution of magnesium bicarbonate and/or calcium bicarbonate is obtained by filtration.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US08721998B2 |
|---|
| Quelldatensatz | uspto-grants-2014_05 |
|---|
| ORD ID | ord-588e1c15a0e24ca79b7e32fabfc72018 |
|---|
| Quellennotiz | uspto-grants-2014_05 |
|---|