Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Acrylonitrile | HCID 7855 | — |
| Edukt | Butyl Acrylate | HCID 8846 | — |
| Edukt | Sodium Lauryl Sulfate | HCID 3423265 | — |
| Lösungsmittel | Water | HCID 962 | — |
| Produkt | Butyl acrylate acrylonitrile | HCID 168389 | — |
Reaktionsschritte
Into a 2 L reactor equipped with an agitator, a thermometer, a nitrogen gas inlet tube, a dropping funnel, and a reflux condenser, was placed 600 g of distilled water, 0.71 g of sodium dodecyl sulfate as an emulsifier, and as monomers, 70 g of acrylonitrile and 30 g of n-butyl acrylate, and the reactor was nitrogen-purged while the reaction mixture was being stirred at 80° C. Next, 1.6 g of 4,4′-azobis(4-cyanovaleric acid) as a polymerization initiator together with 30 g of distilled water was added into the reactor, and a reaction was initiated. Stirring was performed at 80° C. for 10 hours, and an acrylonitrile/n-butyl acrylate random copolymer was produced with a conversion rate of monomers of 89%. GPC measurement confirmed that Mw=472,000, Mn=214,000, and Mw/Mn=2.21.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US07094833B2 |
|---|
| Quelldatensatz | uspto-grants-2006_08 |
|---|
| ORD ID | ord-9012a462bfb94024b4c6414b67674db0 |
|---|
| Quellennotiz | uspto-grants-2006_08 |
|---|