Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Di-n-butyldilauryltin | HCID 9809426 | — |
| Edukt | Mercaptoisocyanate | HCID 22024120 | — |
| Produkt | Azelaic Acid | HCID 2266 | — |
Reaktionsschritte
About 50 grams of the mercaptoisocyanate solution prepared in Example 1 along with 0.01 g of dibutyltin dilaurate should be added to about 40 grams of the above prepared polyester and heated for about 3 hours at 100° C. to form a polyester having reactive mercapto groups.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US04255541 |
|---|
| Quelldatensatz | uspto-grants-1981_03 |
|---|
| ORD ID | ord-1d9a4d1467d44e169ad50c717548d628 |
|---|
| Quellennotiz | uspto-grants-1981_03 |
|---|