Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | 1-Butanol | HCID 263 | — |
| Edukt | Azobisisobutyronitrile | HCID 6547 | — |
| Edukt | Acrylic Acid | HCID 6581 | — |
| Edukt | Methyl Methacrylate | HCID 6658 | — |
| Edukt | Isobutyl Methacrylate | HCID 7352 | — |
| Edukt | Ethyl Acrylate | HCID 8821 | — |
| Lösungsmittel | O-Xylene | HCID 7237 | — |
| Produkt | Tall-oil rosin | HCID 90895 | — |
Reaktionsschritte
A mixture of 64 parts of xylene and 16 parts of n-butanol was heated to 90° C. in the same flask as used in Production Example 1. To this was added dropwise a mixture of 25.0 parts of isobutyl methacrylate, 33.0 parts of ethyl acrylate, 22.7 parts of methyl methacrylate, 19.3 parts of acrylic acid and 2 parts of azobisisobutyronitrile at a constant rate over 3 hours. After the addition, the mixture was kept at the same temperature for 30 minutes. Then a solution of 0.2 parts of azobisisobutyronitrile in 16 parts of xylene and 4 parts of n-butanol was added dropwise at a constant rate over 30 minutes. Thereafter the reaction mixture was kept at the same temperature for 2 hours. A resin solution called Varnish D having 49.5% solids, a viscosity of 7.8 poise and a resin acid number of 150 was obtained.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US05880173 |
|---|
| Quelldatensatz | uspto-grants-1999_03 |
|---|
| ORD ID | ord-96fc53d191fc4c5c96c21764b248891c |
|---|
| Quellennotiz | uspto-grants-1999_03 |
|---|