Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Methacrylic Acid | HCID 4093 | — |
| Edukt | Styrene | HCID 7501 | — |
| Edukt | Ammonium Persulfate | HCID 62648 | — |
| Edukt | Sodium | HCID 5360545 | — |
| Edukt | Methacrylic acid ethylene oxide | HCID 21880491 | — |
| Lösungsmittel | Water | HCID 962 | — |
| Produkt | Methacrylic acid ethylene oxide | HCID 21880491 | — |
| Produkt | Styrene methacrylic acid sodium | HCID 69484178 | — |
Reaktionsschritte
A reaction vessel equipped with a stirring bar and a thermometer was charged with 683 parts of water, 11 parts of a sodium salt of sulfuric acid ester of methacrylic acid-ethylene oxide adduct (ELEMINOL RS-30, manufactured by Sanyo Chemical Industries, Ltd.), 138 parts of styrene, 138 parts of methacrylic acid, and 1 part of ammonium persulfate, and the resulting mixture was stirred for 15 minutes at 400 rpm, to thereby obtain a white emulsion. The obtained emulsion was heated to have the system temperature of 75° C., and was then allowed to react for 5 hours. To the resultant, 30 parts of a 1% ammonium persulfate aqueous solution was added, followed by aging for 5 hours at 75° C., to thereby obtain an aqueous dispersion liquid of a vinyl resin (a copolymer of styrene/methacrylic acid/sodium salt of sulfuric acid ester of methacrylic acid ethylene oxide adduct), i.e., Particle Dispersoin Liquid 1.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US08932789B2 |
|---|
| Quelldatensatz | uspto-grants-2015_01 |
|---|
| ORD ID | ord-fb600c0fd4914c428e52ddaf9fc9fb9e |
|---|
| Quellennotiz | uspto-grants-2015_01 |
|---|