Zurück
HuagongsheHuagongshe Chemie-Druckbericht · Nur für Forschungszwecke
HRID 1439142Erstellt: 25. Oktober 2026

Formaldehyde → Urea, polymer with formaldehyde and 1,3,5-triazine-2,4,6-triamine

https://huagongshe.com/reaction/1439142

Reaktionsgleichung

Beteiligte Stoffe

RolleNameHCIDEinwaage
EduktFormaldehydeHCID 712—
EduktSulfur DioxideHCID 1119—
EduktUreaHCID 1176—
EduktMelamineHCID 7955—
LösungsmittelWaterHCID 962—
LösungsmittelO-XyleneHCID 7237—
ProduktUrea, polymer with formaldehyde and 1,3,5-triazine-2,4,6-triamineHCID 168250—

Reaktionsbedingungen

Temperatur65 °C

Reaktionsschritte

A urea-formaldehyde-melamine prepolymer solution is prepared from 165 grams of 37% aqueous formaldehyde, 45 grams of water, 89 grams of urea and 1 gram of melamine, adjusted to pH 9.3 and heated for 1 hour at 65° C. 170 grams of this prepolymer solution are emulsified in a solution of 6 grams of Tetronic 1502 dissolved in 100 grams of xylene, and 0.06 milliequivalents of sulfur dioxide (about 4 normal in xylene solution) is added, resulting in an exothermic reaction. After stirring for 1 hour, the solvent dispersion has little or no precipitate. Without any preliminary phase separation, the product is mixed with water to give about 16% total solids, and this "aqueous redispersion" is steam distilled under high-shear agitation to yield a product free of residual xylene, closely resembling that described in Example 1. A paper coating prepared as described in Example 1 has a scatter coefficient of about 4,000 cm2 /gram.

Herkunft & Nachweise

DOI10.6084/m9.figshare.5104873.v1
PatentnummerUS04058434
Quelldatensatzuspto-grants-1977_11
ORD IDord-09fdc8cd40fb42a9b47e86718552c886
Quellennotizuspto-grants-1977_11