[C:1]([O:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12][CH2:13][CH2:14][CH2:15][CH2:16][CH2:17][CH2:18][CH2:19][CH2:20][CH2:21][CH2:22][CH2:23][CH3:24])(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:25]([OH:30])(=[O:29])[C:26]([CH3:28])=[CH2:27].SCCO>>[C:1]([O:6][CH2:7][CH2:8][CH2:9][CH2:10][CH2:11][CH2:12][CH2:13][CH2:14][CH2:15][CH2:16][CH2:17][CH2:18][CH2:19][CH2:20][CH2:21][CH2:22][CH2:23][CH3:24])(=[O:5])[C:2]([CH3:4])=[CH2:3].[C:25]([OH:30])(=[O:29])[C:26]([CH3:28])=[CH2:27]The resultant product contained 24.64 percent by weight of a 1:2 copolymer of stearyl methacrylate (SMA) and methacrylic acid (MAA), 0.61 percent residual SMA; less than 0.02 percent residual MAA; no initiator; less than 0.05 percent 2-mercaptoethanol; and had a bulk viscosity at 25° C. of about 4000-5000 centipoise. When the product was diluted to 10% polymeric solids with further oil, the solution had a viscosity at 25° C. of 36-46 centipoise.