Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Ammonia | HCID 222 | — |
| Edukt | Urea | HCID 1176 | — |
| Edukt | Titanium Tetrachloride | HCID 24193 | — |
| Lösungsmittel | Water | HCID 962 | — |
| Produkt | Titanium Tetrachloride | HCID 24193 | — |
| Produkt | Titanium hydroxide | HCID 88494 | — |
Reaktionsschritte
An aqueous solution of titanium tetrachloride was prepared in the same manner as Example 1. 197 mL of ion-exchanged water was added to the aqueous solution of titanium tetrachloride, and then 283 g of aqueous solution of urea having a concentration of 30% by weight and kept at 80° C. was added over 100 minutes. After the resulting solution was heated and refluxed for 10 hours, an aqueous solution of ammonia having a concentration of 5% by weight was added to the solution so that it had a pH of 10. The solution was washed with water until chlorine was no longer detected, thereby providing a slurry of titanium hydroxide. Then, using the slurry of titanium hydroxide, a slurry of titanium oxide was prepared in the same manner as Example 8 (the first process). The titanium oxide was found to have an average particle diameter of 0.03 μm by electron microscopic measurement.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US08431109B2 |
|---|
| Quelldatensatz | uspto-grants-2013_04 |
|---|
| ORD ID | ord-99de2fd08752481eb0f8be35ef11c8be |
|---|
| Quellennotiz | uspto-grants-2013_04 |
|---|