Phenol → (1,1'-Biphenyl)-2,3'-diol

HRID 2049919
Drucken

Reaktionsgleichung

Reaktionsgleichung von HRID 2049919
C1([OH:7])C=CC=CC=1.[CH:8](Cl)(Cl)[CH:9](Cl)Cl.[CH:14]1[CH:19]=[C:18]([C:20]2[CH:25]=[CH:24][CH:23]=[C:22]([OH:26])[CH:21]=2)[C:17]([OH:27])=[CH:16][CH:15]=1>>[CH:14]1[CH:19]=[C:18]([C:20]2[CH:25]=[CH:24][CH:23]=[C:22]([OH:26])[CH:21]=2)[C:17]([OH:27])=[CH:16][CH:15]=1.[OH:7][C:23]1[CH:22]=[CH:21][C:20]([CH2:18][CH2:19][C:14]2[CH:15]=[CH:16][C:17]([OH:27])=[CH:9][CH:8]=2)=[CH:25][CH:24]=1
KomponentenVersuchsvorschriftAufarbeitungQuellen und NachweiseNotizen zur Reaktion

Komponenten

5

Edukt 3

HCID 996PhenolHCID 65911,1,2,2-TetrachloroethaneHCID 33665(1,1'-Biphenyl)-2,3'-diol

Produkt 2

HCID 33665(1,1'-Biphenyl)-2,3'-diolHCID 801521,2-Bis(4-hydroxyphenyl)ethane

Versuchsvorschrift

The inherent viscosity of the polyesters determined at 30° C., in a solvent combination of 60 parts by weight phenol and 40 parts by weight sym-tetrachloroethane at a concentration of 0.5 g per dl., is at least about 0.5 and is preferably at least about 0.7. The selection of acid and diphenol components is made so that the polyester preferably has a glass transition temperature of at least 100° C., a viscosity at 320° C. determined in a capillary rheometer at a shear rate of 100 sec-1 of less than 105 poise and a melting point less than about 350° C. An especially preferred group of polyarylene esters comprises those polyesters obtained by condensation of a diphenol comprising at least 90 mol percent 1,2-bis(4-hydroxyphenyl)ethane and a dicarboxylic acid comprising at least 67 mol percent isophthalic acid. Of this preferred group, one of the more preferred combinations is obtained from 1,2-bis(4-hydroxyphenyl)ethane and isophthalic acid without additional components. The preferences are based on the availability and cost of the acid as well as on the desirable glass transition and melting points of the resulting polyesters. Since molding cycles are preferably rapid, it is desirable that a crystalline polyester crystallize in the short period during which the polymer is cooling in the mold. Thus a molding material for uses where high temperature dimensional stability is important, needs to have a rapid rate of crystallization. The glass transition temperature, the melting point and the rate of crystallization can be determined by means of differential scanning calorimetry as described in copending application Ser. No. 709,469, filed July 28, 1976, now U.S. Pat. No. 4,102,864, which methods are hereby incorporated by reference.

Aufarbeitung

  1. customat 320° C.

Quellen und Nachweise

ORD-Eintrag
ord-e009c75b9b95463aa7f6417a6783bd83
Quelldatensatz
uspto-grants-1980_04
DOI
10.6084/m9.figshare.5104873.v1
Patentnummer
US04199493

Notizen zur Reaktion

Auf dieser SeiteKomponentenVersuchsvorschriftAufarbeitungQuellen und NachweiseNotizen zur Reaktion