| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Methanol | HCID 887 | — |
| Edukt | 1,1'-Dimethyl 2,2'-(1,2-diazenediyl)bis(2-methylpropanoate) | HCID 75763 | — |
| Edukt | 4-Ethenylphenyl acetate | HCID 75821 | — |
| Edukt | 2-Ethyl-2-methacryloyloxyadamantane | HCID 9813645 | — |
| Lösungsmittel | Acetone | HCID 180 | — |
| Lösungsmittel | Isopropanol | HCID 3776 | — |
| Produkt | 2-ethyl-2-adamantyl Methacrylate p-acetoxystyrene | HCID 86587147 | — |
Reaktionsschritte
Into a flask were charged 39.7 g (0.16 mol) of 2-ethyl-2-adamantyl methacrylate, 103.8 g (0.64 mol) of p-acetoxystyrene and 265 g of isopropanol, and the mixture was heated up to 75° C. under a nitrogen atmosphere. Into this solution was dropped a solution prepared by dissolving 11.05 g (0.048 mol) of dimethyl 2,2′-azobis(2-methylpropionate) in 22.11 g of isopropanol. The mixture was aged for about 0.3 hours at 75° C., and for about 12 hours under reflux, then, diluted with acetone. The reaction solution was poured into a large amount of methanol to precipitate a polymer which was filtrated. The amount of the resulted copolymer of 2-ethyl-2-admantyl methacrylate and p-acetoxystyrene was 250 g (weight of wet cake containing methanol).
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US06689531B2 |
|---|
| Quelldatensatz | uspto-grants-2004_02 |
|---|
| ORD ID | ord-b566d380804248c1b39787bf7b7a0245 |
|---|
| Quellennotiz | uspto-grants-2004_02 |
|---|