Reaktionsgleichung

Beteiligte Stoffe

RolleNameHCIDEinwaage
EduktPropylene OxideHCID 6378—
EduktMethyl MethacrylateHCID 6658—
EduktPhthalic AnhydrideHCID 6811—
EduktBenzoyl PeroxideHCID 7187—
EduktSodium HydroxideHCID 14798—
EduktSodium orthosilicateHCID 26051—
ProduktSodium silicate methyl methacrylate propylene oxideHCID 86738390—

Reaktionsschritte

About 50 parts by weight of an aqueous sodium silicate solution containing about 10% Na2O and 25% SiO2 by weight, 25 parts by weight of methyl methacrylate, 10 parts by weight of propylene oxide, 2 parts by weight of phthalic anhydride, 5 parts by weight of sodium hydroxide and 0.5 parts by weight of benzoyl peroxide are thoroughly mixed thereby producing an emulsion. The mixture is reacted at ambient temperature and pressure for 1 to 24 hours thereby producing a poly(sodium silicate-methyl methacrylate-propylene oxide) copolymer emulsion.

Herkunft & Nachweise

DOI10.6084/m9.figshare.5104873.v1
PatentnummerUS04353999