Reaktionsgleichung
[CH2:1]=[CH:2][CH:3]=[CH2:4].[C:5](#N)[CH:6]=[CH2:7].[C:9](O)(=O)[CH:10]=[CH2:11]>>[CH3:7][C:6]1[CH2:5][CH2:4][C@@H:3]([C:10]([CH3:11])=[CH2:9])[CH2:2][CH:1]=1Komponenten
4
Versuchsvorschrift
Photopolymer plates based on a terpolymer of butadiene, acrylonitrile, and acrylic acid were processed as in Example 1 with this solvent. Wash time for this type plate in this solution was 18 minutes. Again the plate quality was superior to that obtained with perchloroethylene under the same conditions. No phasing of this solution was observed.
Aufarbeitung
- washWash time for this type plate in this solution
- customthat obtained with perchloroethylene under the same conditions