EduktMethylphosphonic acidHCID 13818—
EduktAluminum HydroxideHCID 10176082—
LösungsmittelWaterHCID 962—
ProduktAluminum methylphosphonateHCID 2335494657,7%

Reaktionsbedingungen

Temperatur160 °C

Reaktionsschritte

0.780 g of aluminum hydroxide, 1.47 g of methylphosphonic acid, and 6.64 g of water were mixed and stirred for 1 hour. Then the mixture was placed in an internal cylinder of Teflon in a stainless steel pressure-resistant vessel, which was placed in turn in a constant-temperature bath, and the mixture in the vessel was heated under autogenous pressure at 160° C. for 48 hours. After cooling to room temperature, suspended needle crystals were scooped out, washed with water, and dried in air, to obtain 0.97 g of aluminum methylphosphonate. The product gave essentially the same powder X-ray diffraction pattern as that in Example 4, and the product also contained a phase that gave essentially the same powder X-ray diffraction pattern as that in Example 1.

Herkunft & Nachweise

DOI10.6084/m9.figshare.5104873.v1
PatentnummerUS05595952
Quelldatensatzuspto-grants-1997_01
ORD IDord-c1761b9049854099ae1e723c113b9ac4
Quellennotizuspto-grants-1997_01