Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Ethylene carbonate | HCID 7303 | — |
| Katalysator | Sodium metaborate | HCID 145326 | — |
| Lösungsmittel | Diethylene Glycol | HCID 8117 | — |
| Produkt | Carbon Dioxide | HCID 280 | 17,8% |
| Produkt | Ethylene carbonate | HCID 7303 | 100% |
Reaktionsschritte
A 50:1 mole ratio of ethylene carbonate to diethylene glycol is heated with stirring under a nitrogen atmosphere for 45 hours at 160° C. using 1.0 percent sodium metaborate as catalyst to give 100 percent ethylene carbonate conversion to a poly(alkylene carbonate) polyol with 17.8 percent carbon dioxide. The catalyst is removed as in Example 1.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US04709069 |
|---|
| Quelldatensatz | uspto-grants-1987_11 |
|---|
| ORD ID | ord-ebfbf94f624d48f287be4b52346279fa |
|---|
| Quellennotiz | uspto-grants-1987_11 |
|---|