Reaktionsgleichung
C(=O)([O-])[O-:2].[Mg+2:5].[S:6](=[O:8])=[O:7]>>[S:6](=[O:2])([OH:8])[O-:7].[Mg+2:5].[S:6](=[O:2])([OH:8])[O-:7]Komponenten
3
Versuchsvorschrift
According to the invention a method of recovering magnesia from magnesium carbonate containing raw material includes the steps of forming a slurry of uncalcined raw material, heating the slurry to a temperature between 40° and 90° C., treating the slurry with sulphur dioxide to form soluble magnesium bisulphite, separating undissolved impurities from the solution of magnesium bisulphite, precipitating magnesium sulphite from the solution, separating the precipitate from the mother liquor and recovering magnesia from the separated precipitate.
Aufarbeitung
- customof forming a slurry of uncalcined raw material
- temperatureheating the slurry to a temperature between 40° and 90° C.
Quellen und Nachweise
- ORD-Eintrag
- ord-e2ec1990de354442a2347f9662ca4e4b
- Quelldatensatz
- uspto-grants-1979_05
- Patentnummer
- US04154802
Verknüpfte Notizen