Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Sodium Carbonate | HCID 10340 | — |
| Edukt | 2,5-Dihydrofuran | HCID 15570 | — |
| Edukt | Carbonate Ion | HCID 19660 | — |
| Edukt | Sodium orthosilicate | HCID 26051 | — |
| Edukt | Barium | HCID 5355457 | — |
| Edukt | Sodium | HCID 5360545 | — |
| Edukt | Magnesium | HCID 5462224 | — |
| Katalysator | Chromium | HCID 23976 | — |
| Katalysator | Copper | HCID 23978 | — |
| Katalysator | Zinc | HCID 23994 | — |
| Lösungsmittel | Water | HCID 962 | — |
| Produkt | Gamma-Butyrolactone | HCID 7302 | — |
| Produkt | Furan | HCID 8029 | — |
| Produkt | 2,3-Dihydrofuran | HCID 70934 | — |
Reaktionsschritte
In a manner similar to that described in Example 1 15 mL/h of 2,5-dihydrofuran and 32 mL/h of water were passed at 220° C. over 149 g of a catalyst containing copper and magnesium on silicon dioxide (composition: copper, calculated as Cuo: 43.0 wt %; magnesium, calculated as MgO: 18.0 wt %; silicate, calculated as SiO2 : 35.0 wt %; barium, calculated as BaO: 1 wt %; chromium, calculated as Cr2O3 : 0.6 wt %; zinc, calculated as ZnO: 0.4 wt %; sodium, calculated as Na2O: 0.2 wt %; the remainder being predominantly carbonate; all data based on the total weight of the catalyst; prepared by concurrent precipitation from a solution of the metal salts and sodium silicate (waterglass) with sodium carbonate, drying of the precipitate, extrusion to extrudates using talcum as molding auxiliary and calcination at 500° C., and reduction in a manner similar to that described in Example 1). At a conversion of 97%, γ-butyrolactone was obtained with a selectivity of 85% (2,3-dihydrofuran: 1.4%; furan: 3%; tetrahydrofuran: 9%; n-butanol: 1%; remainder: small amounts of various non-analyzed low-boiling fractions).
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US05646307 |
|---|
| Quelldatensatz | uspto-grants-1997_07 |
|---|
| ORD ID | ord-143e9122d6c04040b24e3efe7bb16b45 |
|---|
| Quellennotiz | uspto-grants-1997_07 |
|---|