Reaktionsgleichung
[CH:1]1[C:6]([C:7]2[CH:12]=[CH:11][C:10]3[C:13]([O:15][C:16](=[O:17])[C:9]=3[CH:8]=2)=[O:14])=[CH:5][C:4]2[C:18]([O:20][C:21](=[O:22])[C:3]=2[CH:2]=1)=[O:19].[CH:23]1[C:28]([NH2:29])=[CH:27][C:26]([C:30]([F:33])([F:32])[F:31])=[C:25]([C:34]2[CH:39]=[CH:38][C:37]([NH2:40])=[CH:36][C:35]=2[C:41]([F:44])([F:43])[F:42])[CH:24]=1>CN1C(=O)CCC1>[CH:1]1[C:6]([C:7]2[CH:12]=[CH:11][C:10]3[C:13]([O:15][C:16](=[O:17])[C:9]=3[CH:8]=2)=[O:14])=[CH:5][C:4]2[C:18]([O:20][C:21](=[O:22])[C:3]=2[CH:2]=1)=[O:19].[CH:38]1[C:37]([NH2:40])=[CH:36][C:35]([C:41]([F:44])([F:42])[F:43])=[C:34]([C:25]2[CH:24]=[CH:23][C:28]([NH2:29])=[CH:27][C:26]=2[C:30]([F:31])([F:32])[F:33])[CH:39]=1Komponenten
4
Edukt 2
Produkt 1
Reagenzien, Katalysatoren, Lösungsmittel 1
Versuchsvorschrift
A solution of polyamic acid was prepared at room temperature by combining 4.853 grams of 6FDA, 3.200 grams of BPDA, 6.967 grams of TFMB and 62.1 grams of NMP with good mixing. The amic acid solution was diluted to 10.9% solids, then cast on a silicon wafer by spin coating, and imidized by a heat treatment up to a maximum temperature of 300° C. to produce a coating having a thickness of 2.1 microns. The refractive index was determined in the same manner as in Example 1 and is reported in Table I.
Aufarbeitung
- customA solution of polyamic acid was prepared at room temperature
- customimidized by a heat treatment up to a maximum temperature of 300° C.
- customto produce a coating
Quellen und Nachweise
- ORD-Eintrag
- ord-b37d2905e38146968b8c5b5cf707a1a6
- Quelldatensatz
- uspto-grants-1997_07
- Patentnummer
- US05649045