Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Methanol | HCID 887 | — |
| Edukt | 4-Methylpyridine | HCID 7963 | — |
| Edukt | 1-Decene | HCID 13381 | — |
| Edukt | HCID 178418361 | HCID 178418361 | — |
| Edukt | HCID 178418416 | HCID 178418416 | — |
| Katalysator | Cobaltous octanoate | HCID 6451291 | — |
| Produkt | Methyl undecanoate | HCID 15607 | — |
Reaktionsschritte
After placing 0.008 mole of cobalt octanoate in a stainless steel autoclave having a capacity of 100 ml, 1 hour's stirring was conducted at a temperature of 160°C while applying first a pressure of 10 Kg/cm2 with hydrogen and then applying a pressure of 150 Kg/cm2 to thereby prepare a catalyst. Meanwhile, after placing 0.65 mole of decene-1, 0.08 mole of γ-picoline and 0.5 mole of methanol in a stainless steel autoclave having a capacity of 300 ml, a pressure of 30 Kg/cm2 was applied thereto with carbon monoxide. Subsequently, the previously prepared catalyst was added to the contents of the latter autoclave, and 5 hours' reaction of the mixture was effected at a temperature of 160°C under the same pressure, or 30 Kg/cm2. The yield rate of methyl undecanoate obtained through distillation of the reacted mixture was 35%.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US03946055 |
|---|
| Quelldatensatz | uspto-grants-1976_03 |
|---|
| ORD ID | ord-4fdf14b52da541549fff5462de71571f |
|---|
| Quellennotiz | uspto-grants-1976_03 |
|---|