Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | 2-Phenylethanol | HCID 6054 | — |
| Katalysator | Silver | HCID 23954 | — |
| Lösungsmittel | Water | HCID 962 | — |
| Produkt | Phenylacetaldehyde | HCID 998 | 67% |
Reaktionsschritte
The same installation as in Example 1 is used. A catalyst comprising 82 parts of silver crystals of particle sizes from 0.1 to 2.5 mm is introduced, as a homogeneous bed, into the reactor. The height of the catalyst bed is 30 mm. Using a similar method to Example 1, a mixture of 150 parts of 2-phenylethanol and 60 parts of water with 210 parts of air is passed per hour over the catalyst at 540° C. and 1.1 bar. The residence time is 0.07 second and the throughput 0.2 tonne/m2.h. 99 parts of phenylacetaldehyde (in the form of a 73 percent strength by weight organic phase) are obtained per hour, corresponding to a yield of 67% of theory. The conversion is 78 percent and the space-time yield is 5 grams of phenylacetaldehyde per cm3 of catalyst volume per hour.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US04224254 |
|---|
| Quelldatensatz | uspto-grants-1980_09 |
|---|
| ORD ID | ord-b2a8411aac314ac2b525c7037d0c0abb |
|---|