Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Carbon Dioxide | HCID 280 | — |
| Edukt | 2-Vinylpyridine | HCID 7521 | — |
| Edukt | Diphenylmethane | HCID 7580 | — |
| Edukt | Naphthalene potassium | HCID 66602812 | — |
| Lösungsmittel | Acetone | HCID 180 | — |
| Lösungsmittel | Tetrahydrofuran | HCID 8028 | — |
| Produkt | Potassium diphenylmethane | HCID 66720999 | — |
Reaktionsschritte
First, poly(2-vinylpyridine) homopolymer was prepared by using 2-vinylpyridine (2VP) monomer at −78° C. and under high vacuum (10−6 torr) in the solvent of THF for 30 min. The temperature of −78° C. is maintained by adding dry ice in a constant-temperature bath with acetone, and measured with a thermometer for low temperature. The initiator of potassium diphenylmethane (DPM-K) was prepared by reacting potassium-naphthalene (K-NaPh) ion solution with diphenylmethane, and diluted to appropriate concentration using a distribution device connected to vacuum line. The initiator was divided into glass ampoules and stored in a low temperature refrigerator.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US07425593B2 |
|---|
| Quelldatensatz | uspto-grants-2008_09 |
|---|
| ORD ID | ord-d0efe49e78ac475b9514f01985d6775d |
|---|
| Quellennotiz | uspto-grants-2008_09 |
|---|