HuagongsheHuagongshe Chemie-Druckbericht · Nur für Forschungszwecke
Sodium Hydroxide → Sodium orthosilicate
Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|---|---|---|
| Edukt | Sodium Hydroxide | HCID 14798 | — |
| Edukt | Sodium Silicate | HCID 23266 | — |
| Produkt | Sodium orthosilicate | HCID 26051 | — |
Reaktionsschritte
50 kg of water glass having an SiO2/Na2O of 3.45 and an active substance content of 36.1% (grade Na 4/1 from Clariant France S.A.) were admixed with 5.66 kg of sodium hydroxide solution (48% strength) and spray-dried in a laboratory spray dryer (spray tower) from Anhydro to give an amorphous sodium silicate having an active substance content of 84%. 15 kg of the amorphous sodium silicate are heat-treated at 720° C. for 90 min in a muffle furnace (Nabertherm, model W1000/H). The chilled material (about 10 kg) is pulverized using a jaw crusher and a disk mill.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patentnummer | US06743766B1 |
| Quelldatensatz | uspto-grants-2004_06 |
| ORD ID | ord-0759ed3cd03c48a7a5c1814b264c191d |
| Quellennotiz | uspto-grants-2004_06 |