Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Ammonia | HCID 222 | — |
| Edukt | Carbon Dioxide | HCID 280 | — |
| Edukt | Stearic Acid | HCID 5281 | — |
| Edukt | Zinc Oxide | HCID 3007857 | — |
| Lösungsmittel | Water | HCID 962 | — |
| Produkt | Stearic Acid | HCID 5281 | — |
| Produkt | Zinc Stearate | HCID 11178 | — |
| Produkt | Zinc Oxide | HCID 3007857 | — |
Reaktionsschritte
130 kg of zinc oxide is dispersed in a rotor-stator shear machine with 16 liters of 25% aqueous ammonia in 480 liters of cold water with simultaneous introduction of gaseous carbon dioxide. Simultaneously, 900 kg of molten stearic acid is emulsified at 80° C. in 180 liters of water and to the emulsion there is added 36 liters of 25% aqueous ammonia. Both dispersions are fed at 80° C. through correspondingly adjusted dosing pumps to a rotor-stator shear machine likewise heated to 80° C., so that stoichiometric amounts are reacted per unit of time. From the 130 kg of zinc oxide and 900 kg of stearic acid (saponification number=204) there is formed 1000 kg of zinc stearate. The pasty zinc stearate drawn off from the rotor-stator shear machine has a water content of about 45%. It is fed directly to a flowing air dryer in which it is dried to a water content of 0.2%. The end product is a finely granular, extremely pure, electrolyte-free zinc stearate.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US04376079 |
|---|
| Quelldatensatz | uspto-grants-1983_03 |
|---|
| ORD ID | ord-548ecfa34cb84a7d8c942fa974dd25bb |
|---|
| Quellennotiz | uspto-grants-1983_03 |
|---|