HuagongsheHuagongshe Chemie-Druckbericht · Nur für Forschungszwecke
HRID 370515Erstellt: 24. Oktober 2026
N-vinyl-2-pyrrolidone → N-vinylpyrrolidone triphenyltin chloride
https://huagongshe.com/de/reaction/370515
Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | N-vinyl-2-pyrrolidone | HCID 6917 | — |
| Edukt | Triphenyltin Chloride | HCID 12540 | — |
| Lösungsmittel | O-Xylene | HCID 7237 | — |
| Produkt | N-vinylpyrrolidone triphenyltin chloride | HCID 86740183 | — |
Reaktionsschritte
The same reactor as used in Example 1 was charged with 30 g of N-vinylpyrrolidone, 104 g of triphenyltin chloride and 200 g of xylene, and the mixture was stirred at 50° C. for 2 hours to form an N-vinylpyrrolidone/triphenyltin chloride adduct. Then, 50 g of butyl acrylate, 16 g of octyl acrylate and 0.5 g of benzoyl peroxide were added, and with stirring, the mixture was heated to 75° C. At this temperature, 0.2 g of benzoyl peroxide was added three times at intervals of 3 hours, and the polymerization reaction was carried out for a total of 12 hours to give an N-coordinated-triphenyltin-containing copolymer solution having a molecular weight of 77,000 (to be referred to as a copolymer solution [A-18]). This copolymer solution was used directly as an antifouling agent.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US04526932 |
|---|
| Quelldatensatz | uspto-grants-1985_07 |
|---|
| ORD ID | ord-8a58580ccd064a9c91bd6696538e305f |
|---|
| Quellennotiz | uspto-grants-1985_07 |
|---|