Zurück
HuagongsheHuagongshe Chemie-Druckbericht · Nur für Forschungszwecke
HRID 371780Erstellt: 25. Oktober 2026

Formaldehyde → Crl-8131

https://huagongshe.com/reaction/371780

Reaktionsgleichung

Beteiligte Stoffe

RolleNameHCIDEinwaage
EduktFormaldehydeHCID 712—
EduktSulfuric AcidHCID 1118—
EduktUreaHCID 1176—
EduktTriethanolamineHCID 7618—
EduktCrl-8131HCID 24751—
EduktSorbitan mono-(9Z)-9-octadecenoateHCID 9920342—
EduktSpan #80 (Sorbitan monooleate)HCID 70693544—
EduktHCID 178435162HCID 178435162—
KatalysatorTitanium oxide (Ti3O)HCID 162651—
LösungsmittelWaterHCID 962—
LösungsmittelO-XyleneHCID 7237—
ProduktCrl-8131HCID 24751—
ProduktUrea formaldehyde foamHCID 62705—

Reaktionsschritte

A urea-formaldehyde prepolymer solution is prepared by heating an aqueous solution of two-hundred-twenty grams of 37% formaldehyde and 82 grams of urea, adjusted to pH 8 with triethanolamine, at 70° C for one hour. Fifty grams of this prepolymer solution are mixed with thirty grams of a 50% by weight dispersion of titanium dioxide in distilled water, and adjusted to pH 6 with dilute sulfuric acid. The aqueous dispersion is emulsified in a solution of six grams of Pluronic L122, three grams of sorbitan monooleate (commerically available as Span 80 from ICI America) and 1.5 grams of a poly(oxyethylene)-poly(oxypropylene) block copolymer with 30% poly(oxyethylene) and a molecular weight of about 2500 (commercially available as Pluronic L 63) in one-hundred grams of xylene to yield a water-in-oil emulsion. This is treated with four milliliters of a 50% by weight solution of monobutyl acid phosphate in toluene and stirred for two hours.

Herkunft & Nachweise

DOI10.6084/m9.figshare.5104873.v1
PatentnummerUS04087581
Quelldatensatzuspto-grants-1978_05
ORD IDord-b9e5ab78aa404bacaa0993020cdab82a
Quellennotizuspto-grants-1978_05