Styrene → Butyl prop-2-enoate;styrene

https://huagongshe.com/de/reaction/384583

Reaktionsgleichung

Beteiligte Stoffe

RolleNameHCIDEinwaage
EduktStyreneHCID 7501—
EduktButyl AcrylateHCID 8846—
EduktPotassium PersulfateHCID 24412—
EduktPotassiumHCID 5462222—
LösungsmittelWaterHCID 962—
ProduktButyl prop-2-enoate;styreneHCID 168422—

Reaktionsbedingungen

Temperatur60 °C

Reaktionsschritte

In a 200-liter reactor equipped with a stirrer, a cooling apparatus, a condenser and a monomer supplying tube, 5 parts by weight of butylacrylate, 15 parts by weight of styrene, 0.2 parts by weight of triallyl isocyanurate, 140 parts by weight of ion-exchanged water and 1.0 parts by weight of potassium rosinate are added and mixed. The temperature is raised to 60° C. with stirring. After 10 minutes from the time of reaching 60° C., 0.25 parts by weight of potassium persulfate dissolved in deionized water is added thereto to initiate polymerization. The temperature of the reactor is maintained at 70° C. for 60 minutes. The polymerization is carried out at 70° C. for an additional 30 minutes to give an inner core of butylacrylate-styrene copolymer.

Herkunft & Nachweise

DOI10.6084/m9.figshare.5104873.v1
PatentnummerUS08367770B2
Quelldatensatzuspto-grants-2013_02
ORD IDord-6308c29c53df4acabed5aeb9c47e1454