O[C:2]1[CH:7]=[CH:6][C:5]([C:8]2([C:18]3[CH:23]=[CH:22][C:21](O)=[CH:20][CH:19]=3)C3C=CC=CC=3C(=O)O2)=[CH:4][CH:3]=1.[CH2:25]([CH:27]1[O:29][CH2:28]1)Cl>>[C:5]1([C:8]2[C:18]3[CH:19]=[CH:20][CH:21]=[CH:22][C:23]=3[O:29][C:28]=2[C:27]2[CH:4]=[CH:3][CH:2]=[CH:7][CH:25]=2)[CH:6]=[CH:7][CH:2]=[CH:3][CH:4]=1Komponenten
3
Versuchsvorschrift
(A-1) 159 g of 3,3-bis(4-hydroxyphenyl)-2-benzofuran-1-on, 426.6 g of epichlorohydrin, and 160 g of a 50% alkali aqueous solution are mixed in a 1 L flask and then reacted together at 95° C. for 1 hour to form a bisphenylbenzofuran-type epoxy resin. 215 g of the bisphenylbenzofuran-type epoxy resin is mixed with 450 mg of triethylbenzylammoniumchloride, 100 mg of 2,6-diisobutylphenol, and 72 g of acrylic acid. The mixture is heated and completely dissolved at a temperature ranging from 90 to 120° C., while air is blown therein at a speed of 25 Ml per minute.
Aufarbeitung
- customreacted together at 95° C. for 1 hour
Quellen und Nachweise
- ORD-Eintrag
- ord-80bee22462ef451986276d8676dcb69f
- Quelldatensatz
- uspto-grants-2013_09
- Patentnummer
- US08530537B2
Verknüpfte Notizen
Wird geladen…