Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Phosphoric Acid | HCID 1004 | — |
| Edukt | Phosphate | HCID 1061 | — |
| Edukt | Zirconium | HCID 23995 | — |
| Produkt | Zirconium phosphate | HCID 160986 | — |
Reaktionsschritte
A zirconium phosphate film was prepared by adding a stoichometric amount of phosphate in the form of phosphoric acid to a solution of zirconium bound to PEI. The solution was then spin coated onto a glass slide and thermally treated at 1° C. to 120° C. with a dwell time of 30 minutes followed by heating to 350° C. at 1° C./minute with a dwell time of 30 minutes followed by heating to 450° C. at 1° C./minute with a dwell time of 1 hour and then cooling to 25° C.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US08530554B1 |
|---|
| Quelldatensatz | uspto-grants-2013_09 |
|---|
| ORD ID | ord-cf4b6531eeb34d11a932e26327e1f566 |
|---|
| Quellennotiz | uspto-grants-2013_09 |
|---|