Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Urea | HCID 1176 | — |
| Edukt | Ethylene Oxide | HCID 6354 | — |
| Edukt | Propylene Oxide | HCID 6378 | — |
| Edukt | Diammonium hydrogen phosphate | HCID 24540 | — |
| Edukt | 2,3-Bis(1-phenylethyl)phenol | HCID 19010394 | — |
| Lösungsmittel | Water | HCID 962 | — |
| Produkt | Styrene | HCID 7501 | — |
| Produkt | Ethyl Acrylate | HCID 8821 | — |
| Produkt | Butyl Acrylate | HCID 8846 | — |
| Produkt | Methylolmethacrylamide | HCID 70208 | — |
Reaktionsschritte
5 parts of sodium polyacrylate (molecular weight about 200,000) are dissolved in 277 parts of water. 5 parts of the oxyalkylation product obtained by reacting 1 mole of di-(α-phenylethyl)-phenol first with 7 moles of propylene oxide and then with 20 moles of ethylene oxide, 10 parts of urea and 3 parts of diammonium phosphate are added to the solution. After a brief period, a homogeneous mixture is obtained, to which 500 parts of gasoline (boiling range 140° - 200° C) and 200 parts of a 40% strength aqueous dispersion of a copolymer of 65 parts of butyl acrylate, 24 parts of styrene, 6 parts of ethyl acrylate and 5 parts of N-methylolmethacrylamide are added, with vigorous stirring (3,000 rmp). A very stable oil-in-water emulsion is obtained, which is particularly suitable for use as a carrier for organic pigments.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US04064309 |
|---|
| Quelldatensatz | uspto-grants-1977_12 |
|---|
| ORD ID | ord-98873e09020145e3b723efc4ce3ef548 |
|---|
| Quellennotiz | uspto-grants-1977_12 |
|---|