Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Phenol | HCID 996 | — |
| Edukt | Phosphoric Acid | HCID 1004 | — |
| Edukt | Oleic Acid | HCID 445639 | — |
| Produkt | Hydroxyphenylstearic acid | HCID 67710449 | — |
Reaktionsschritte
A 500-ml autoclave was charged with 166 g of commercial oleic acid (product of Nippon Oils & Fats Co., Ltd.), 169 g of phenol (product of Katayama Kagaku Kogyo K.K.), 6.6 g of activated clay (Nippon Kassei Hakudo K.K.), and 0.13 g of 85% aqueous phosphoric acid (product of Katayama Kagaku Kogyo K.K.). After purging the autoclave with nitrogen gas, the contents were allowed to react by heating at 200° C. for 4 hours. After completion of the reaction, the activated clay was filtered off and the unreacted phenol was distilled away at 80°-100° C., 3 mmHg to yield a yellow viscous reaction product in an amount of 224 g.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US04888132 |
|---|
| Quelldatensatz | uspto-grants-1989_12 |
|---|
| ORD ID | ord-c1c552b8069745d8a6d1ddec01b86e24 |
|---|
| Quellennotiz | uspto-grants-1989_12 |
|---|