Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Isoprene | HCID 6557 | — |
| Edukt | Styrene | HCID 7501 | — |
| Edukt | 1,3-Butadiene | HCID 7845 | — |
| Lösungsmittel | Methanol | HCID 887 | — |
| Produkt | Isoprene butadiene | HCID 168288 | — |
Reaktionsschritte
Into a dried pressure vessel purged with nitrogen, 80 L of cyclohexane solvent and 0.17 L of sec-butyllithium initiator (10% by mass solution in cyclohexane) were charged. After raising the temperature to 50° C., 3.9 L of styrene was added to allow the polymerization to proceed for 3 h. Then, the polymerization was allowed to proceed for 4 h after adding a mixed liquid of 12.1 L of isoprene and 10.9 L of butadiene and further for 3 h after adding 3.9 L of styrene. The resultant reaction liquid was poured into 80 L of methanol, and the precipitated solid matter was separated by filtration and dried at 50° C. for 20 h, to obtain a polystyrene block-poly(isoprene/butadiene) block-polystyrene block, triblock copolymer.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US09102849B2 |
|---|
| Quelldatensatz | uspto-grants-2015_08 |
|---|
| ORD ID | ord-1d887dd659494004bc27ecf4f7ff803a |
|---|
| Quellennotiz | uspto-grants-2015_08 |
|---|