Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Diphenylmethane diisocyanate | HCID 7570 | — |
| Edukt | Tetrahydrofuran | HCID 8028 | — |
| Edukt | Di-n-butyldilauryltin | HCID 9809426 | — |
| Edukt | Diisocyanatotoluene | HCID 12905475 | — |
| Produkt | Adipic Acid | HCID 196 | — |
| Produkt | 1,4-Butanediol | HCID 8064 | — |
Reaktionsschritte
0.5 g of dibutyltin dilaurate was added to a 60% strength by weight solution of 112.0 g of toluylene diisocyanate and 158.3 g of diphenylmethane 4,4'-diisocyanate in tetrahydrofuran, and the mixture was then heated to 60° C. At this temperature, a 60% strength by weight solution of 390 g of a polyesterol obtained from 1,4-butanediol and adipic acid and having a molecular weight of 1000, 167.5 g of a polyesterol obtained from 1,6-hexanediol, adipic acid and terephthalic acid, 29.4 g of polydimethylsiloxane having hydroxyl functional groups and a molecular weight of 900, 3.17 g of trimethylolpropane, 3.13 g of methyldiethanolamine, 72 g of diethoxylated bisphenol A and 27 g of 1,6-hexanediol in tetrahydrofuran was metered in over 2 hours.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US05922469 |
|---|
| Quelldatensatz | uspto-grants-1999_07 |
|---|
| ORD ID | ord-df212db813d946ecbd3c218005d55494 |
|---|
| Quellennotiz | uspto-grants-1999_07 |
|---|