Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | 1,5-Dihydroxynaphthalene | HCID 6749 | — |
| Edukt | O-Xylene | HCID 7237 | — |
| Edukt | Piperidine | HCID 8082 | — |
| Edukt | EP-302 | HCID 62790 | — |
| Lösungsmittel | Dichloromethane | HCID 6344 | — |
| Produkt | Bisphenol A | HCID 6623 | — |
Reaktionsschritte
This comparative example illustrates the Tg enhancement provided by a relatively bulky linking compound that has been referred to in several patents relating to ED paints. 72.7 Parts EPON 829 and 14.8 parts 1,5-dihydroxynaphthalene were combined neat and reacted overnight at 158° C., then diluted with 28.9 parts mixed xylenes. The resulting dark brown, viscous reaction product solution contained 72.5% solids and had an epoxy equivalent weight of 423 (perchloric acid-tetrabutyl ammonium iodide titration). 19.06 Parts of the reaction product solution were combined with 0.30 parts piperidine and 54.6 parts of xylene:methylene chloride solution, then analyzed using dynamic mechanical analysis. A measured Tg of 134° C. was obtained. This Tg value is 20° C. greater than that obtained when bisphenol A is substituted for such linking compound.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US04822464 |
|---|
| Quelldatensatz | uspto-grants-1989_04 |
|---|
| ORD ID | ord-94bf5411f9564b1b97813c84ef8389ff |
|---|
| Quellennotiz | uspto-grants-1989_04 |
|---|