Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|
| Edukt | Dibutyl Phthalate | HCID 3026 | — |
| Edukt | Ethylene Oxide | HCID 6354 | — |
| Edukt | Propylene | HCID 8252 | — |
| Lösungsmittel | O-Xylene | HCID 7237 | — |
| Produkt | Phthalic Anhydride | HCID 6811 | — |
| Produkt | 1,4-Butanediol | HCID 8064 | — |
Reaktionsschritte
320 parts of a 40% xylene solution of dihydroxyethylenepropylene copolymer (molecular weight; 8,000, propylene content; 50%, prepared by hydroxyethylating both terminals of the ethylene-propylene copolymer as produced by known living anionic polymerization with ethyleneoxide) and 460 parts of a 40% dibutyl phthalate solution of polyester obtained from 1,4-butanediol and phthalic anhydride (equivalent weight ratio; 41/40, molecular weight; 8,000) were fed into a four-mouthed reaction vessel fitted with a powerful stirrer, a temperature sensor, a condenser and a material charging inlet and stirred for one hour at 100° C. for homogenization. Afterwards, 4.3 parts of hexamethylene diisocyanate was added thereto and stirred for one hour at 120° C., and 0.02 part of dibutyl tin dilaurate was further added thereto and reacted until the NCO content became 0.05 or less (generally, for five hours) to obtain a 40% solvent solution of component (2)(i).
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|
| Patentnummer | US05130359 |
|---|
| Quelldatensatz | uspto-grants-1992_07 |
|---|
| ORD ID | ord-45beeec7efef45469c6d040426e9f5a4 |
|---|
| Quellennotiz | uspto-grants-1992_07 |
|---|