2-Hydroxyethyl acrylate → Urethane acrylate
Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|---|---|---|
| Edukt | 2-Hydroxyethyl acrylate | HCID 13165 | — |
| Edukt | Isophorone diisocyanate | HCID 169132 | — |
| Edukt | Methionin AL | HCID 446793 | — |
| Katalysator | Zinc | HCID 23994 | — |
| Produkt | Urethane acrylate | HCID 21863578 | — |
Reaktionsschritte
Metal-containing polyol from Example 6 was used to prepare a zinc salt urethane diacrylate oligomer based on isophorone diisocyanate and hydroxyethyl acrylate. Isophorone diisocyanate (IPDI, 135.41 g) was added to the polyol which was diluted with 25% ethoxylated trimethyolpropane triacrylate (polyol, 2000.0 g; SR454, 100.0 g) over 2 hours at 60° C., followed by addition of hydroxyethyl acrylate (70.8 g). The reaction mixture was kept at 90° C. for 4 hour. A viscous liquid resin was obtained. The final product is light yellow and hazy liquid. The viscosity @ 60° C. is only 920 cps.
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patentnummer | US06380278B1 |
| Quelldatensatz | uspto-grants-2002_04 |
| ORD ID | ord-b6dd8695493f4b7fac48b9d994f55ba6 |
| Quellennotiz | uspto-grants-2002_04 |