[CH2:1]=[CH2:2].[C:3]([O:6][CH:7]=[CH2:8])(=[O:5])[CH3:4].[CH:9]([O:11][C:12](=[O:15])[CH2:13][Cl:14])=[CH2:10]>>[C:3]([O:6][CH:7]=[CH2:8])(=[O:5])[CH3:4].[CH:9]([O:11][C:12](=[O:15])[CH2:13][Cl:14])=[CH2:10].[CH2:1]=[CH2:2]The aqueous copolymer dispersion was prepared in an analogous manner to example 11, but by carrying out the polymerization with a modified monomer mixture at an ethylene pressure of 5 atmospheres. A mixture of 764 g of vinyl acetate and 76 g of monochloroacetic acid vinyl ester was added to the polymerization mixture at room temperature and after the polymerization had started a mixture of 6880 g of vinyl acetate and 688 g of monochloroacetic acid vinyl ester was introduced by pumping over a period of 6 hours. The dispersion obtained of a copolymer of vinyl acetate/monochloroacetic acid vinyl ester/ethylene had a solids content of 51% by weight and a latex viscosity of 23 poises.