Versuchsvorschrift

In a one-liter autoclave were charged 400 ml of toluene as a polymerization solvent, 0.001 moles of perbutyl neodecanoate as a polymerization initiator, 0.42 moles of N-methylmaleimide, and 4.05 moles of isobutene, and the mixture was subjected to polymerization reaction under a polymerization condition at a polymerization temperature of 60° C. for a polymerization time of 5 hours, to obtain N-methylmaleimide-isobutene alternating copolymer. The thus obtained N-methylmaleimide-isobutene alternating copolymer had a weight average molecular weight (Mw) (as reduced into standard polystyrene) of 165,000 and an Mw/Mn of 2.6.

Aufarbeitung

  1. customthe mixture was subjected to polymerization reaction under a polymerization condition at a polymerization temperature of 60° C. for a polymerization time of 5 hours

Quellen und Nachweise

ORD-Eintrag
ord-aecbe2064ad24c798523ce957c5cb948
Quelldatensatz
uspto-grants-2006_02
Patentnummer
US07001967B2

Verknüpfte Notizen

Wird geladen…