HuagongsheHuagongshe Chemie-Druckbericht · Nur für Forschungszwecke
Pyromellitic dianhydride → Acetic Anhydride
Beteiligte Stoffe
| Rolle | Name | HCID | Einwaage |
|---|---|---|---|
| Edukt | Pyromellitic dianhydride | HCID 6966 | — |
| Edukt | Dimethylacetamide | HCID 31374 | — |
| Edukt | 5,5'-Bi-2-benzofuran-1,1',3,3'-tetrone | HCID 75494 | — |
| Produkt | Acetic Anhydride | HCID 7918 | — |
| Produkt | 3-Methylpyridine | HCID 7970 | — |
Reaktionsschritte
Polymer was made at room temperature by adding 3,4′-ODA, PPD, BPDA, and PMDA with stirring in DMAc in quantities to make polymers with compositions between 5 and 14 mole % BPDA and between 5 and 21 mole % PPD. The remaining monomers were PMDA as the dianhydride and 3,4′-ODA as the diamine. The polymers were each cast on a substrate and converted in a bath of 50 volume % acetic anhydride and 50 volume % beta-picoline, at room temperature, to form a gel film. The gel film was restrained and heated in an oven to dry and cure at 300° C. for 60 minutes, and then heated in 400° C. oven for 5 minutes. The properties were as follows:
Herkunft & Nachweise
| DOI | 10.6084/m9.figshare.5104873.v1 |
|---|---|
| Patentnummer | US06956098B2 |
| Quelldatensatz | uspto-grants-2005_10 |
| ORD ID | ord-4934ef4e9f334061aa924d7e01e66895 |
| Quellennotiz | uspto-grants-2005_10 |