[O-2].[Sm+3:2].[O-2].[O-2].[Sm+3].[N+:6]([O-:9])([OH:8])=[O:7]>>[N+:6]([O-:9])([O-:8])=[O:7].[Sm+3:2].[N+:6]([O-:9])([O-:8])=[O:7].[N+:6]([O-:9])([O-:8])=[O:7]Slightly excess samarium oxide was dissolved in concentrated nitric acid under heating to effect the reaction. After 1 hour, the reaction liquid was filtered and the filtrate was cooled to precipitate crystalline samarium nitrate. Yield: 60%.