Cobalt → cobalt (III) hexammine sulphate

HRID 1387190
Print

Reaction equation

HRID 1387190 reaction equation
[Co:1].[S:2]([OH:6])([OH:5])(=[O:4])=[O:3].[CH:7](=[NH:13])[CH2:8][CH2:9][CH2:10][CH2:11][CH3:12].[S:14]([O-:18])([O-:17])(=[O:16])=[O:15].[NH4+].[NH4+].[Co+3]>>[S:2]([O-:6])([O-:5])(=[O:4])=[O:3].[CH:7](=[NH:13])[CH2:8][CH2:9][CH2:10][CH2:11][CH3:12].[Co+3:1].[S:14]([O-:18])([O-:17])(=[O:16])=[O:15].[S:2]([O-:6])([O-:5])(=[O:4])=[O:3].[Co+3:1]
ParticipantsProcedureWorkupSources & evidenceReaction notes

Participants

5

Reactant 4

HCID 104730CobaltHCID 105146Cobaltic cationHCID 6097028Ammonium SulfateHCID 86757217Hexammine sulphate

Product 1

HCID 86757216cobalt (III) hexammine sulphate

Procedure

In a process for producing cobalt metal powder from nickel-cobalt sulphides comprising leaching said nickel-cobalt sulphides in an ammoniacal ammonium sulphate solution under an elevated pressure of an oxygen bearing gas, at a temperature of at least 80° C., with an effective ammonia to metals mole ratio in the range of 5:1 to 6.5:1 to oxidize the nickel and cobalt sulphides to sulphates, and to produce an ammoniacal ammonium sulphate leach liquor in which dissolved cobalt is predominantly in the (III) oxidation state, and an ammoniacal ammonium sulphate leach residue containing a cobalt (III) hexannmine sulphate-calcium sulphate double salt, separating the ammoniacal ammonium sulphate leach liquor from the ammoniacal ammonium sulphate leach residue, saturating the ammoniacal ammonium sulphate leach liquor with an effective amount of anydrous ammonia and cooling the ammoniated leach liquor to below 50° C. to precipitate the triple salt of cobalt (III) hexammine supbate, nickel (II) hexammine sulphate and ammonium sulphate, recovering the precipitated triple salt from the leach liquor, repulping the triple salt with an effective amount of water to selectively leach nickel(II) hexammine sulphate and to produce a crystalline cobalt (III) hexammine sulphate with a Co:Ni ratio of at least 100:1 and a nickel enriched leach liquor, dissolving the cobalt (III) hexammine sulphate in hot ammonium sulphate solution, and cooling the solution to precipitate recrystallized cobalt (III) hexammine sulphate having a Co:Ni ratio of at least about 1000:1 and treating the recrystallized cobalt (III) hexammine sulphate to produce cobalt metal therefrom, the improvement comprising:

Workup

  1. customseparating the ammoniacal ammonium sulphate leach liquor from the ammoniacal ammonium sulphate leach residue
  2. concentrationsaturating the ammoniacal ammonium sulphate leach liquor with an effective amount of anydrous ammonia
  3. temperaturecooling the ammoniated leach liquor to below 50° C.
  4. customto precipitate the triple salt of cobalt (III) hexammine supbate, nickel (II) hexammine sulphate and ammonium sulphate
  5. customrecovering the precipitated triple salt from the leach liquor

Sources & evidence

ORD record
ord-0039413553eb487b9f079f83668c2355
Source dataset
uspto-grants-2001_07
DOI
10.6084/m9.figshare.5104873.v1
Patent number
US06267800B1

Reaction notes

On this pageParticipantsProcedureWorkupSources & evidenceReaction notes